https://www.avient.com/products/fiber-line-engineered-fiber-solutions/fiber-line
Back
Home //
Products //
Engineered Fiber Solutions //
Performance Fiber Conversion Calculator
https://www.avient.com/company/policies-and-governance/california-transparency-act-disclosure
Home //
Innovating Tomorrow's Materials Solutions Today //
Policies and Governance
https://www.avient.com/knowledge-base/article/need-fresh-color-ideas-differentiate-your-mens-grooming-packaging
We can help you position your products at the front of consumers’ minds with winning solutions – fast.
https://www.avient.com/knowledge-base/ebook/smart-colorants-making-most-color
Choosing the best solution for your material, process, and end use application means evaluating different technologies against your particular requirements and goals, and then avoiding common pitfalls.
https://www.avient.com/knowledge-base/article/new-horizons-fiber-optic-cable
The case for high-performance material solutions
https://www.avient.com/sites/default/files/2022-05/Compensation Committee Charter (REV 10-2019).pdf
Review and Discuss the CD&A and Compensation Committee Report
With the assistance of management and any outside advisers the Committee deems
appropriate (a) review and discuss with management the Company’s disclosures in the
CD&A, and, based on this review, make a recommendation as to whether to include it in the
Company’s annual report on Form 10-K and proxy statement relating to the Company’s
annual meeting of shareholders, and (b) prepare a Compensation Committee Report for
inclusion in the Company’s proxy statement or other applicable SEC filings.
4
Board Reports and Annual Evaluation
Regularly report the Committee’s activities and any recommendations to the Board in such
manner and at such times as the Committee or the Board deems appropriate.
• Conduct an annual evaluation of the Committee’s performance.
https://www.avient.com/sites/default/files/2020-09/lubrione-processing-guide.pdf
PROBLEM CAUSE SOLUTION
Incomplete Fill Melt and/or mold
temperature too cold
Shot Size
• Increase nozzle and barrel temperatures
• Increase mold temperature
• Increase injection speed
• Increase pack and hold pressure
• Increase nozzle tip diameter
• Check thermocouples and heater bands
• Enlarge or widen vents and increase number of vents
• Check that vents are unplugged
• Check that gates are unplugged
• Enlarge gates and/or runners
• Perform short shots to determine fill pattern and verify
proper vent location
• Increase wall thickness to move gas trap to parting line
• Increase cushion
Brittleness Melt temperature too low
Degraded/Overheated material
Gate location and/or size
• Increase melt temperature
• Increase injection speed
• Measure melt temperature with pyrometer
• Decrease melt temperature
• Decrease back pressure
• Use smaller barrel/excessive residence time
• Relocate gate to nonstress area
• Increase gate size to allow higher flow speed and
lower molded-in stress
Fibers on Surface
(Splay)
Melt temperature too low
Insufficient packing
• Increase melt temperature
• Increase mold temperature
• Increase injection speed
• Increase pack and hold pressure, and time
Sink Marks Part geometry too thick
Melt temperature too hot
Insufficient material volume
• Reduce wall thickness
• Reduce rib thickness
• Decrease nozzle and barrel temperatures
• Increase shot size
• Increase injection rate
• Increase packing pressure
Flash Injection pressure too high
Excess material volume
Melt and/or mold
temperature too hot
• Decrease injection pressure
• Increase clamp pressure
• Decrease injection speed
• Increase transfer position
• Decrease pack pressure
• Decrease shot size
• Decrease injection speed
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
• Decrease screw speed
TROUBLESHOOTING RECOMMENDATIONS
PROBLEM CAUSE SOLUTION
Excessive Shrink Too much orientation • Increase packing time and pressure
• Increase hold pressure
• Decrease melt temperature
• Decrease mold temperature
• Decrease injection speed
• Decrease screw rpm
• Increase venting
• Increase cooling time
Not Enough Shrink Too little orientation • Decrease packing pressure and time
• Decrease hold pressure
• Increase melt temperature
• Increase mold temperature
• Increase injection speed
• Increase screw rpm
• Decrease cooling time
Burning Melt and/or mold
temperature too hot
Mold design
Moisture
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
• Clean, widen and increase number of vents
• Increase gate size or number of gates
• Verify material is dried at proper conditions
Nozzle Drool Nozzle temperature too hot • Decrease nozzle temperature
• Decrease back pressure
• Increase screw decompression
• Verify material has been dried at proper conditions
Weld Lines Melt front temperatures
too low
• Increase pack and hold pressure
• Increase melt temperature
• Increase vent width and locations
• Increase injection speed
• Decrease injection speed
• Increase gate size
• Perform short shots to determine fill pattern and verify
proper vent location
• Add vents and/or false ejector pin
• Move gate location
Warp Excessive orientation
• Increase cooling time
• Increase melt temperature
• Decrease injection pressure and injection speed
• Increase number of gates
Sticking in Mold Cavities are overpacked
Part is too hot
• Decrease injection speed and pressure
• Decrease pack and hold pressure
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
• Increase cooling time
• Increase draft angle
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
TROUBLESHOOTING RECOMMENDATIONS
Note: These are general processing conditions.
Values reported as “typical” or stated without a range do not state minimum or maximum properties; consult your
sales representative for property ranges and min/max specifications.
AVIENT MAKES NO WARRANTIES, EXPRESS
OR IMPLIED, INCLUDING, BUT NOT LIMITED TO, IMPLIED WARRANTIES OF MERCHANTABILITY AND FITNESS FOR A PARTICULAR PURPOSE, either with respect to the information or products reflected by the
information.
https://www.avient.com/sites/default/files/2020-09/edgetek-processing-guide.pdf
PROBLEM CAUSE SOLUTION
Excessive Shrink Too much orientation • Increase packing time and pressure
• Increase hold pressure
• Decrease melt temperature
• Decrease mold temperature
• Decrease injection speed
• Decrease screw rpm
• Increase venting
• Increase cooling time
Not Enough Shrink Too little orientation • Decrease packing pressure and time
• Decrease hold pressure
• Increase melt temperature
• Increase mold temperature
• Increase injection speed
• Increase screw rpm
• Decrease cooling time
Burning Melt and/or mold
temperature too hot
Mold design
Moisture
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
• Clean, widen and increase number of vents
• Increase gate size or number of gates
• Verify material is dried at proper conditions
Nozzle Drool Nozzle temperature too hot • Decrease nozzle temperature
• Decrease back pressure
• Increase screw decompression
• Verify material has been dried at proper conditions
Weld Lines Melt front temperatures
too low
• Increase pack and hold pressure
• Increase melt temperature
• Increase vent width and locations
• Increase injection speed
• Decrease injection speed
• Increase gate size
• Perform short shots to determine fill pattern and verify
proper vent location
• Add vents and/or false ejector pin
• Move gate location
Warp Excessive orientation
• Increase cooling time
• Increase melt temperature
• Decrease injection pressure and injection speed
• Increase number of gates
Sticking in Mold Cavities are overpacked
Part is too hot
• Decrease injection speed and pressure
• Decrease pack and hold pressure
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
• Increase cooling time
• Increase draft angle
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
TROUBLESHOOTING RECOMMENDATIONS
PROBLEM CAUSE SOLUTION
Incomplete Fill Melt and/or mold
temperature too cold
Shot Size
• Increase nozzle and barrel temperatures
• Increase mold temperature
• Increase injection speed
• Increase pack and hold pressure
• Increase nozzle tip diameter
• Check thermocouples and heater bands
• Enlarge or widen vents and increase number of vents
• Check that vents are unplugged
• Check that gates are unplugged
• Enlarge gates and/or runners
• Perform short shots to determine fill pattern and verify
proper vent location
• Increase wall thickness to move gas trap
to parting line
• Increase cushion
Brittleness Melt temperature too low
Degraded/Overheated material
Gate location and/or size
• Increase melt temperature
• Increase injection speed
• Measure melt temperature with pyrometer
• Decrease melt temperature
• Decrease back pressure
• Use smaller barrel/excessive residence time
• Relocate gate to nonstress area
• Increase gate size to allow higher flow speed and lower
molded-in stress
Fibers on Surface
(Splay)
Melt temperature too low
Insufficient packing
• Increase melt temperature
• Increase mold temperature
• Increase injection speed
• Increase pack and hold pressure, and time
Sink Marks Part geometry too thick
Melt temperature too hot
Insufficient material volume
• Reduce wall thickness
• Reduce rib thickness
• Decrease nozzle and barrel temperatures
• Increase shot size
• Increase injection rate
• Increase packing pressure
Flash Injection pressure too high
Excess material volume
Melt and/or mold
temperature too hot
• Decrease injection pressure
• Increase clamp pressure
• Decrease injection speed
• Increase transfer position
• Decrease pack pressure
• Decrease shot size
• Decrease injection speed
• Decrease nozzle and barrel temperatures
• Decrease mold temperature
• Decrease screw speed
TROUBLESHOOTING RECOMMENDATIONS
www.avient.com
Copyright © 2020, Avient Corporation.
Values reported as “typical” or stated without a range do not state minimum or maximum properties; consult your
sales representative for property ranges and min/max specifications.
AVIENT MAKES NO WARRANTIES, EXPRESS
OR IMPLIED, INCLUDING, BUT NOT LIMITED TO, IMPLIED WARRANTIES OF MERCHANTABILITY AND FITNESS FOR A PARTICULAR PURPOSE, either with respect to the information or products reflected by the
information.
https://www.avient.com/sites/default/files/2020-08/2020-hammerhead-application-install-guide.pdf
Values reported as “typical” or stated without a range do not state minimum or maximum properties; consult your
sales representative for property ranges and min/max specifications.
AVIENT MAKES NO WARRANTIES, EXPRESS
OR IMPLIED, INCLUDING, BUT NOT LIMITED TO, IMPLIED WARRANTIES OF MERCHANTABILITY AND FITNESS FOR A PARTICULAR PURPOSE, either with respect to the information or products reflected by the
information.
To learn more about Avient’s advanced composite solutions,
contact Avient at +1.844.4AVIENT
www.avient.com
https://www.avient.com/sites/default/files/2023-12/Polystrand Thermoplastic Composite Panel Application _ Install Guide.pdf
Values reported as “typical” or stated without a range do not state minimum or maximum properties; consult your
sales representative for property ranges and min/max specifications.
AVIENT MAKES NO WARRANTIES, EXPRESS
OR IMPLIED, INCLUDING, BUT NOT LIMITED TO, IMPLIED WARRANTIES OF MERCHANTABILITY AND FITNESS FOR A PARTICULAR PURPOSE, either with respect to the information or products reflected by the
information.
To learn more about our advanced composite solutions,
contact Avient at 1.844.4AVIENT or visit www.avient.com.